Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 394 kV/mm | 10000 kV/in | 0.25 inch electrodes in dry air @25°C; ASTM D149-81 |
DuPont Teijin Films Melinex® S Polyester Film, 48 Gauge Melinex® S is a general purpose film which combines excellent handling characteristics with a slightly hazy appearance. It is available in specific thicknesses from 48 - 500 gauge, and is used for .. |