Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 102 kV/mm | 2580 kV/in | Z Direction; IPC-TM-650 2.5.6.2 |
Rogers Corporation XT/duroid™ 8100 0.002" Woven Glass Reinforced Thermoplastic Circuit Material XT/duroid™ 8100 woven glass reinforced thermoplastic circuit materials provide an excellent solution for printed circuit board applications used in demanding environmental conditions. XT/duroid 81.. |
|||
Dielectric Strength | 102 kV/mm | 2600 kV/in | |
Saint-Gobain CHR® 2345-1 Polyimide Film Backing Silicone Adhesive Pressure Sensitive Tape Description: Polyimide films are employed because of their extreme heat resistance. Service temperatures range from -100°F to 500°F (-73°C to 260°C). These flame retardant films exhibit .. |
|||
Dielectric Strength | 102 kV/mm | 2600 kV/in | ASTM D-149 |
Saint-Gobain Norton® T-100 Virgin Skived PTFE Film (0.003" thick) T-100/T-200 Features/Benefits: Outstanding heat and chemical resistance; High dielectric strength; Anti-stick properties; Can be chemically etched for bondability; Applications include laminate rele.. |
|||
Dielectric Strength | 102 kV/mm | 2600 kV/in | |
Saint-Gobain CHR® K250 Polyimide Film Backing Silicone Adhesive Pressure Sensitive Tape Description: Polyimide films are employed because of their extreme heat resistance. Service temperatures range from -100°F to 500°F (-73°C to 260°C). These flame retardant films exhibit .. |
|||
Dielectric Strength | 102 kV/mm | 2590 kV/in | 4.5 mil film; ASTM D149 |
3M Dyneon™ FEP 6307Z Fluorinated Ethylene Propylene Fluorothermoplastic Granules Dyneon FEP 6307Z is offered for extrusion, injection molding and transfer molding for the wire and cable and chemical process industries. Their distinguishing features include: Excellent electrical .. |