Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Dielectric Strength = 13.9 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 13.9 kV/mm
353 kV/in
Short Time; ASTM D149
Plenco 08235 Polyester BMC, Compression Molded
PLENCO 08235 is a renumber of PlasGlas 20315. PLENCO 08235 is a 15% glass-filled polyester bulk molding compound characterized as a flame-retardant, medium strength electrical grade. It is suitable ..
Dielectric Strength 13.9 kV/mm
353 kV/in
Short Time; ASTM D149
Plenco 4466 Phenolic, Granular, Compression Molded
PLENCO 04466 is a heat resistant, mineral and flock filled phenolic molding compound, offering excellent mechanical strength and cosmetic properties. UL recognized under component file E40654. 04466..
Dielectric Strength 13.9 kV/mm
354 kV/in
ASTM D149
Arlon LW401C##FR-P1 0.040" (1.02 mm) Self-Fusing Silicone Tape (Triangular, Unsupported)
Description: 1 inch wide, 40 mil thick, Brown, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll length..
Dielectric Strength 13.9 kV/mm
353 kV/in
Short Time; ASTM D149
Plenco 7321 Phenolic, Nodular, Compression Molded
PLENCO 07321 is an organic fiber reinforced phenolic molding compound, offering improved mechanical strength and excellent dimensional stability. Type ASTM 5948 CFI-5, and UL recognized under compon..