Electrical Properties Metric English Comments
Dielectric Strength 530 kV/mm
13500 kV/in
Dow CYCLOTENE™ 3022-35 Bisbenzocyclobutene (BCB) Electronic Resin
This product was developed for use as spin-on dieletric materials in microelectronic fabrication.Information provided by Dow
Dielectric Strength 530 kV/mm
13500 kV/in
Dow CYCLOTENE™ 3022-46 Bisbenzocyclobutene (BCB) Electronic Resin
This product was developed for use as spin-on dieletric materials in microelectronic fabrication.Information provided by Dow
Dielectric Strength 530 kV/mm
13500 kV/in
Dow CYCLOTENE™ 3022-57 Bisbenzocyclobutene (BCB) Electronic Resin
This product was developed for use as spin-on dieletric materials in microelectronic fabrication.Information provided by Dow
Dielectric Strength 530 kV/mm
13500 kV/in
Dow CYCLOTENE™ 3022-63 Bisbenzocyclobutene (BCB) Electronic Resin
This product was developed for use as spin-on dieletric materials in microelectronic fabrication.Information provided by Dow
Dielectric Strength 530 kV/mm
13500 kV/in
Dow CYCLOTENE™ 4022-35 Advanced Electronic Resins (PhotoBisbenzocyclobutene BCB)
CYCLOTENE™ 4022-35 advanced electronic resin is I-line-, G-line-, and broad band-sensitive photopolymer that has been developed for use as a dielectric in thin film microelectronic applications.Inf..
Dielectric Strength 530 kV/mm
13500 kV/in
Dow CYCLOTENE™ 4024-40 Advanced Electronic Resins (PhotoBisbenzocyclobutene BCB)
CYCLOTENE™ 4024-40 advanced electronic resin is I-line-, G-line-, and broad band-sensitive photopolymer that has been developed for use as a dielectric in thin film microelectronic applications.Inf..
Dielectric Strength 530 kV/mm
13500 kV/in
Dow CYCLOTENE™ 4026-46 Advanced Electronic Resins (PhotoBisbenzocyclobutene BCB)
CYCLOTENE™ 4026-46 advanced electronic resin is I-line-, G-line-, and broad band-sensitive photopolymer that has been developed for use as a dielectric in thin film microelectronic applications.Inf..
Dielectric Strength 530 kV/mm
13500 kV/in
Dow CYCLOTENE™ XU35075 Advanced Electronic Resins (PhotoBisbenzocyclobutene BCB)
CYCLOTENE™ XU35075 advanced electronic resin is I-line-, G-line-, and broad band-sensitive photopolymer that has been developed for use as a dielectric in thin film microelectronic applications.Inf..
Dielectric Strength 530 kV/mm
13500 kV/in
Dow CYCLOTENE™ XU35132 Advanced Electronic Resins (PhotoBisbenzocyclobutene BCB)
CYCLOTENE™ XU35132 advanced electronic resin is I-line-, G-line-, and broad band-sensitive photopolymer that has been developed for use as a dielectric in thin film microelectronic applications.Inf..
Dielectric Strength 530 kV/mm
13500 kV/in
Dow CYCLOTENE™ XU35133 Advanced Electronic Resins (PhotoBisbenzocyclobutene BCB)
CYCLOTENE™ XU35133 advanced electronic resin is I-line-, G-line-, and broad band-sensitive photopolymer that has been developed for use as a dielectric in thin film microelectronic applications.Inf..