Electrical Properties Metric English Comments
Dielectric Strength 0.600 kV/mm

@Diameter >=3.00 mm
15.2 kV/in

@Diameter >=0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Parallel; IEC 60243-1; IEC/EN 61212-2 6.1.2.1
Elektro-Isola Etronax MF Phenolic, Cotton Fabric Reinforcement, Brown, Tubes
Description: Mechanical applications. Impact-resistant, noise-reducing and wear-resistant material. Well suited as a low-friction material. High wear resistance in aggressive and dust-filled environ..