Electrical Properties Metric English Comments
Dielectric Strength 14.4 - 15.3 kV/mm
366 - 389 kV/in
ASTM D149-97a
DSM Somos® ProtoGen™ O-XT 18120 Epoxy Resin for Stereolithography, UV Postcure at HOC -2
DescriptionDSM Somos® ProtoGen O-XT 18120 is a liquid photopolymer that produces accurate parts ideal for general purpose applications. ProtoGen resins are the first SL resins to demonstrate diffe..