Electrical Properties Metric English Comments
Dielectric Strength 591 kV/mm
15000 kV/in
Aremco Pyro-Tape™ 682-AR High Temperature Tape Single-layer ultra-high molecular weight polyethylene with a rubber adhesive
Applications Abrasion Resistance Features Low coefficient of friction to reduce wear, scratching and noise. Liners for chutes, rails and slides.