Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 40.0 - 157 kV/mm | 1020 - 4000 kV/in | Average value: 81.5 kV/mm Grade Count:5 |
Overview of materials for Cyclo Olefin Polymer This property data is a summary of similar materials in the MatWeb database for the category "Cyclo Olefin Polymer". Each property range of values reported is minimum and maximum values of appropria.. |