Polymer Property : Dielectric Strength = 1666 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 65.59 kV/mm
1666 kV/in
Saint-Gobain CHR® M797 Polyester Film Backing Natural Rubber Adhesive Pressure Sensitive Tape
Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa..
Dielectric Strength 65.59 kV/mm
1666 kV/in
Saint-Gobain CHR® M803 Polyester Film Backing Silicone Adhesive Pressure Sensitive Tape
Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa..
Dielectric Strength 65.59 kV/mm
1666 kV/in
Saint-Gobain CHR® M815 Polyester Film Backing Silicone Adhesive Pressure Sensitive Tape
Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa..
Dielectric Strength 65.59 kV/mm
1666 kV/in
Saint-Gobain CHR® M827 Polyester Film Backing Silicone Adhesive Pressure Sensitive Tape
Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa..
Dielectric Strength 65.59 kV/mm
1666 kV/in
Saint-Gobain CHR® M897 Polyester Film Backing Natural Rubber Adhesive Pressure Sensitive Tape
Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa..
Dielectric Strength 65.59 kV/mm
1666 kV/in
Saint-Gobain CHR® K100 Polyimide Film Backing Silicone Adhesive Pressure Sensitive Tape
Description: Polyimide films are employed because of their extreme heat resistance. Service temperatures range from -100°F to 500°F (-73°C to 260°C). These flame retardant films exhibit ..