Dielectric Strength 17.18 kV/mm

@Thickness 2.00 mm
436.4 kV/in

@Thickness 0.0787 in
IEC 60243-1
Gromax 1163LL TPE
163LL is medium modulus grade with nominal Durometer hardness of 63D. It contains color stable antioxidants. It can be processed by thermoplastic processing techniques like injection molding and ext..