Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 18.14 kV/mm @Thickness 2.00 mm |
460.8 kV/in @Thickness 0.0787 in |
IEC 60243-1 |
Gromax 1172LL TPE 1172LL is high modulus grade with nominal Durometer hardness of 72D. It contains color stable antioxidants. It can be processed by thermoplastic processing techniques like blow molding grade. Charac.. |