Polymer Property : Dielectric Strength = 19.2 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 19.2 kV/mm

@Thickness 3.20 mm
488 kV/in

@Thickness 0.126 in
in air; ASTM D149
SABIC Innovative Plastics Lexan® 3412R PC (Asia Pacific)
20% GR, provides improved mechanical properties and UL94 V-1 rated at 0.058"". Internal mold release added.
Dielectric Strength 19.2 kV/mm

@Thickness 3.20 mm
488 kV/in

@Thickness 0.126 in
in oil; ASTM D149
SABIC Innovative Plastics LNP THERMOCOMP Lexan_LGN2000 PC (Asia Pacific)
Dielectric Strength 19.2 kV/mm

@Thickness 3.20 mm
488 kV/in

@Thickness 0.126 in
in oil; ASTM D149
SABIC Innovative Plastics NORYL N190X PPE+HIPS (Asia Pacific)
PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0/5VA rated. Dielectric strength. Suitable for E/E market applications.
Dielectric Strength 19.2 kV/mm

@Thickness 3.20 mm
488 kV/in

@Thickness 0.126 in
in oil; ASTM D149
SABIC Innovative Plastics NORYL N190X PPE+PS
PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0/5VA rated. RTI Elec/Imp/Str 95/80/95. Dielectric strength. Suitable for E/E market applications.
Dielectric Strength 19.2 kV/mm
487 kV/in
ACC QGel 310 QSI Quantum Silicones High Strength Gel
QGel 310 is a clear, very soft, tough moderately cross-linked silicone polymer. Silicone gels are used to provide protection from vibration and thermal or mechanical shock. Silicone gels also provid..
Dielectric Strength 19.2 kV/mm

@Thickness 3.20 mm
488 kV/in

@Thickness 0.126 in
in air; ASTM D149
SABIC Innovative Plastics Lexan® 3412R PC
20% GR, provides improved mechanical properties and UL94 V-1 rated at 0.058"". Internal mold release added.