Polymer Property : Dielectric Strength = 190 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 3.50 - 7.48 kV/mm
88.9 - 190 kV/in
Average value: 4.71 kV/mm Grade Count:7
Overview of materials for Silicone Foam
This property data is a summary of similar materials in the MatWeb database for the category "Silicone Foam". Each property range of values reported is minimum and maximum values of appropriate MatW..