Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 20.1 kV/mm | 510 kV/in | ASTM D149 |
Ravago Manufacturing Americas Hylon® N1013HL Nylon 6/6 (DAM) Information provided by Ravago. |
|||
Dielectric Strength | 20.1 kV/mm | 510 kV/in | ASTM D149 |
Ravago Manufacturing Americas Hylon® N1013L Nylon 6/6 (DAM)
(discontinued **) Information provided by Ravago. |
|||
Dielectric Strength | 20.1 kV/mm @Thickness 1.90 mm |
511 kV/in @Thickness 0.0748 in |
|
Momentive Performance Materials RTV627 Dark Gray General Purpose Potting/Encapsulating Compound Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth.. |
|||
Dielectric Strength | 20.1 kV/mm | 510 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PBT GF40 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | 20.1 kV/mm | 510 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PP G/CF40 CC 40% Glass/Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Carbon Fiber Reinforcement, 40% Filler by WeightFeatures: Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | 20.1 kV/mm | 510 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PP GF/M50 CC BK 50% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 50% Filler by WeightFeatures: Chemically CoupledAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | 20.1 kV/mm | 510 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PP LGF50 CC NAT 12mm 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Long Glass Fiber, 50% Filler by WeightFeatures: Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | 20.1 kV/mm | 510 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PP GF50 CC HF BK 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightFeatures: Chemically CoupledAppearance: BlackInformation provided by TP Composites, Inc... |
|||
Dielectric Strength | 20.1 kV/mm | 511 kV/in | ASTM D149-93 |
Saint-Gobain Versilicâ„¢ SPX-70I.B. High Strength Silicone Pressure Tubing Formulation Description: Versilicâ„¢ SPX-70 I.B.: Produced form a proprietary combination of silicone elastomers, Versilicâ„¢ SPX-70 I.B. Tubing optimizes critical physical properties such as tensile st.. |
|||
Dielectric Strength | 20.1 kV/mm | 510 kV/in | |
Tra-Con Tra-Cast 3103 General Purpose Epoxy Casting Compound TRA-CAST 3103 is a low viscosity two-part formulation recommended for general purpose electrical potting and encapsulating application where the combination of good mechanical thermal and electrical.. |
|||
Dielectric Strength | 20.1 kV/mm | 510 kV/in | |
Tra-Con Tra-Cast 3113 General Purpose Epoxy Casting Compound TRA-CAST 3113 is a low viscosity two-part formulation recommended for general purpose electrical potting and encapsulating applications where the combination of good mechanical thermal and electrica.. |
|||
Dielectric Strength | 20.1 kV/mm | 510 kV/in | ASTM D149 |
Arlon 55359R062 62 mil Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PELayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 162 FiberglassThis data represents typical values for the production materi.. |
|||
Dielectric Strength | 20.1 kV/mm | 510 kV/in | ASTM D149 |
Arlon 55589R033 0.033" (0.838 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneLayer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: 162 Style FiberglassAppearance: Red silicone gum and rubber on fiberglass This.. |
|||
Dielectric Strength | 20.1 kV/mm | 511 kV/in | ASTM D149 |
Arlon T2040-B004 0.040" (1.02 mm) Cured Self-Fusing Silicone Rubber Description: 1 inch wide x 40 mil thick, Black, Triangular cross-section, Self-Fusing Silicone TapeDesign/Construction: Interleave: Polyester Product: Cured Self-Fusing Silicone RubberCross-Section:.. |
|||
Dielectric Strength | 20.1 kV/mm | 510 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PP LGF40 CC HS BK 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Heat StabilizerFeatures: Chemically Coupled and Heat StabilizedAppearance: Bla.. |