Electrical Properties Metric English Comments
Dielectric Strength 8.40 kV/mm
213 kV/in
AC 60 Hz; 150°C for 1,000 hrs
Fujipoly Industries Sarcon® 30T Thin-Film TR
Sarcon TR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GTR is a composite of ..
Dielectric Strength 8.40 kV/mm
213 kV/in
Step by Step; ASTM D149
Plenco 6500 Phenolic, Briquette, Injection Molded
PLENCO 06500 is a glass reinforced phenolic molding compound offering improved strength, dimensional stability, and excellent electrical properties. UL recognized under component file E40654. 06500 ..