Electrical Properties Metric English Comments
Dielectric Strength 8.70 kV/mm
221 kV/in
ASTM D149
Proto3000 Duraform® GF Selective Laser Sintering (SLS®) Prototyping Polymer
Description: Glass-filled polyamide (nylon) material for real-world physical testing and functional useFeatures:Excellent mechanical stiffnessElevated temperature resistanceDimensionally stableEasy-..
Dielectric Strength 8.70 kV/mm
221 kV/in
Short Time; Dry; ASTM D149
Resinoid 2215 Phenolic Molding, Cellulose Reinforced
Data provided by the manufacturer.The Resinoid 2000 organic fiber reinforced series compounds feature mechanical strength, dimensional stability, and shock resistance
Dielectric Strength 8.70 kV/mm
221 kV/in
ASTM D149
IDI Composites 46-16-60 Thermoset Polyester, Sheet
TRANSIT - A premium molding compound with excellent resistance to flame and smoke generation, high impact strength, and weatherability.Data provided by the manufacturer.
Dielectric Strength 8.70 kV/mm

@Thickness 1.59 mm
221 kV/in

@Thickness 0.0625 in
100% RH for 96 hours; ASTM D149
Garlock GYLON® 3565 ENVELON® PTFE Gasketing, Glass Microsphere Filled
PTFE with aluminosilicate microsphere filler.Soft, deformable exterior conforms to surface irregularities; ideal for worn, warped or pitted flangesStable blue core improves cold flow resistanceLow b..
Dielectric Strength 8.70 kV/mm
221 kV/in
ac; ASTM D116
CoorsTek AD-995 Alumina (nom. 99.5% Al2O3)
Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
Dielectric Strength 8.70 kV/mm
221 kV/in
ac; ASTM D116
CoorsTek AD-998 Alumina(nom. 99.8% Al2O3)
Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
Dielectric Strength 8.70 kV/mm
221 kV/in
ac; ASTM D116
CoorsTek FG-995 Alumina (nom. 98.5% Al2O3)
Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
Dielectric Strength 8.70 kV/mm
221 kV/in
AC; ASTM D116
CoorsTek PlasmaPure™ Alumina (nom. 99.8% Al2O3)
Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
Dielectric Strength 8.70 kV/mm
221 kV/in
Du-Co Ceramics DC-10-L-3 Steatite
Properties reported below are averages from unglazed specimens. Tests performed to ASTM specifications. Actual values may vary. Information provided by DU-CO Ceramics Company.
Dielectric Strength 8.70 kV/mm
221 kV/in
ASTM D149
3D Systems DuraForm® GF Glass Filled Nylon
For use with all selective laser sintering (SLS®) systems.ApplicationsHousings and enclosuresConsumer sporting goodsAppropriate for low- to mid-volume rapid manufacturingParts requiring machining o..
Dielectric Strength 8.70 kV/mm
221 kV/in
Short Time; Dry; ASTM D149
Resinoid 2020 Phenolic Molding, Fabric Reinforced
Data provided by the manufacturer.The Resinoid 2000 organic fiber reinforced series compounds feature mechanical strength, dimensional stability, and shock resistance
Copyright © lookpolymers.com All Rights Reserved