Electrical Properties Metric English Comments
Dielectric Strength 48.0 - 272 kV/mm

@Temperature 200 - 200 °C
1220 - 6910 kV/in

@Temperature 392 - 392 °F
Average value: 157 kV/mm Grade Count:3
Overview of materials for Polyimide, Thermoset Film
This property data is a summary of similar materials in the MatWeb database for the category "Polyimide, Thermoset Film". Each property range of values reported is minimum and maximum values of appr..