Polymer Property : Dielectric Strength = 279 kV/in
Polymer Property :
Dielectric Strength =
279 kV/in
Product List
Electrical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties
Metric
English
Comments
Dielectric Strength
10.0
-
11.0
kV/mm
254
-
279
kV/in
ASTM D149
Adamas Adalon® 452 PTFE, Mica filler
Information provided by Adamas, HPM