Electrical Properties Metric English Comments
Dielectric Strength 111 kV/mm

@Thickness 3.00 mm
2820 kV/in

@Thickness 0.118 in
ASTM D149
Teknor Apex Chemlon® 104-13 GH Nylon 66, 13% Glass Fiber Reinforced
Notes: Impact Modified; Reinforced with 13% Glass Fibers; Synergistic compound exhibiting impact strength and dimensional stability Features: Good Dimensional stability; Good Processability; Heat St..