Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 3.03 kV/mm

@Thickness 0.930 mm
77.0 kV/in

@Thickness 0.0366 in
3M Scotch-Weld™ 2214 Hi-Dense Epoxy Adhesive
3M™ Scotch-Weld™ Adhesive 2214 Hi-Dense is a deareted version of Scotch-Weld adhesive 2214 regular for use where a very dense, void free bondline is required. One part 250°F (121°C) curing 100% ..
Dielectric Strength 3.03 kV/mm

@Thickness 0.930 mm
77.0 kV/in

@Thickness 0.0366 in
3M Scotch-Weld™ 2214 Regular Epoxy Adhesive
3M™ Scotch-Weld™ Adhesive 2214 Regular is an aluminum filled general purpose product for use in applications where high strength bonds are needed in a temperature range of -53-121°C.One part 250°..