Electrical Properties Metric English Comments
Dielectric Strength 31.1 kV/mm
790 kV/in
ASTM D149
ExxonMobil Santoprene® 111-55 Thermoplastic Elastomer  (discontinued **)
A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range ..
Dielectric Strength 31.1 kV/mm

@Thickness 2.03 mm
790 kV/in

@Thickness 0.0799 in
ASTM D149
ExxonMobil Santoprene® 8221-60 Thermoplastic Rubber  (discontinued **)
A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide..
Dielectric Strength 31.1 kV/mm
790 kV/in
ASTM D149
Arlon R36798T017 0.017" (0.432 mm) Uncured Silicone Rubber with Laminated Tefzel® Substrate  (discontinue
Design/Construction: Liner: PTFE Coated Fiberglass Side 1: Uncured Silicone Rubber Substrate: Laminated Tefzel® Substrate: Treated for adhesionAppearance: Translucent, high viscosity gum on fluoro..
Dielectric Strength 31.1 kV/mm
790 kV/in
2.03 mm; ASTM D149
ExxonMobil Santoprene® 123-40 Thermoplastic Elastomer
A hard, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ran..
Dielectric Strength 31.1 kV/mm

@Thickness 2.03 mm
790 kV/in

@Thickness 0.0799 in
ASTM D149
ExxonMobil Santoprene® 251-92W232 Thermoplastic Elastomer
A hard, colorable, flame retardant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material has good fluid resistance and contains non-ether brominated flame retard..
Dielectric Strength 31.1 kV/mm
790 kV/in
ASTM D149
Arlon 25188T017 Silicone Rubber/Laminated ETFE Film
Liner: 3 mil PTFE coated fiberglass; Side 1: uncured silicone rubber; Substrate: laminated ETFE film, treated for adhesion
Dielectric Strength 31.1 kV/mm
790 kV/in
ASTM D149
Arlon R37208T017 0.017" (0.432 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Liner
Design/Construction: Liner: PTFE Coated Fiberglass Side 1: Uncured Silicone Rubber Substrate: Laminated Tefzel® Substrate: Treated for adhesionThis data represents typical values for the productio..
Dielectric Strength 31.1 kV/mm
790 kV/in
ASTM D149
Arlon 51146R028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone Rubber Interleave: Polyethylene Product Use: Flexible heater insulationAppearance: Red sili..