Electrical Properties Metric English Comments
Dielectric Strength 36.5 kV/mm
927 kV/in
50%RH; IEC 60243-1
DuPont Performance Polymers Zytel® 80G14A NC010A Nylon 66  (Unverified Data**)
14% Glass Reinforced Toughened Polyamide 66 Zytel 80G14A NC010A is a 14% glass fiber reinforced toughened high flow polyamide 66 resin. It offers outstanding performance in injection molding applica..