Polymer Property : Dielectric Strength = 374.9 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 14.76 - 23.62 kV/mm
374.9 - 599.9 kV/in
Arlon Silicone Hose and Duct Material with Polyester Substrate (65390R042)  (discontinued **)
Side one - uncured silicone, 0.005 in., -0.001(0.1 mm, -0.01); Substrate - 6500 Polyester Fabric, 0.038 in. (0.97 mm) nominal; 0.003 in. (0.08 mm) polyethylene interleave; overall thickness 0.042 in..
Dielectric Strength 14.76 - 17.72 kV/mm

@Thickness 3.17 mm
374.9 - 450.1 kV/in

@Thickness 0.125 in
Short time value
Abatron AboCast/AboCure 8109-1
High melting point.Processing: 100/30 pbw; mix at 130-140°C (270 °F); cures in 16 h/120°C (250°F), 10 h/140°C (285°F), 8 h/160°C (320°F), 2 h/ 200°C (390°F).Applications: Heavy duty castin..