Polymer Property : Dielectric Strength = 38.2 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 38.2 kV/mm

@Thickness 1.60 mm
970 kV/in

@Thickness 0.0630 in
ASTM D149
Solvay Specialty Polymers Xydar® MG-350 Liquid Crystal Polymer, Mineral and Glass Filled  (discontinued **)<
XYDAR MG-350 Liquid Crystal Polymer (LCP) is a mineral and glass-filled injection molding grade developed specifically for cost-effective performance in applications where a balance of flatness and ..