Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 38.5 kV/mm | 978 kV/in | IEC 60243-1 |
Lanxess Durethan® DP AKV 30 FN00 000000 Nylon 66, 30% Glass Fiber PA 66, injection molding 30% glass fibers, UL 94 V-0 at 0.4 mm, max. temperature in glow wire test: 960 °C at 0,75 mm, free from halogen and red phosphorous |
|||
Dielectric Strength | 38.5 kV/mm | 978 kV/in | |
Arkema Group Pebax® 5533 SN 01 Polyether Block Amide (PEBA) (Dry) POLYETHER BLOCK AMIDE(PEBA) hardness 55 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: overmolded parts for sport good (Footba.. |
|||
Dielectric Strength | 38.5 kV/mm | 977 kV/in | ASTM D149 |
Arlon 31970XA015 Silicone Rubber Laminate The interleave is 3 mil of polyethylene, side 1 is uncured silicone rubber and the carrier is HDPE. |
|||
Dielectric Strength | 38.5 kV/mm | 978 kV/in | ASTM D149 |
Arlon 48101R008 0.008" (0.203 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: PolyethyleneSide 1: Cured Silicone RubberSubstrate: Style 1080 FiberglassSide 2: Cured Silicone RubberInterleave 2: Polyethylene Product Use: Flexible heater insul.. |