Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 15.0 kV/mm | 382 kV/in | ASTM D149 |
Devcon Brushable Ceramic - Red, Blue Epoxy Precision Repair EpoxyComments: Low-viscosity, alumina-filled, brushable epoxy compound, when applied to a 15-20 mil coating, provides a smooth, protective barrier against wear, abrasion, corrosion,.. |
|||
Dielectric Strength | 15.0 kV/mm | 382 kV/in | ASTM D149 |
Devcon Brushable Ceramic - White Epoxy Precision Repair EpoxyComments: Low-viscosity, alumina-filled, brushable epoxy compound, when applied to a 15-20 mil coating, provides a smooth, protective barrier against wear, abrasion, corrosion,.. |
|||
Dielectric Strength | 15.0 kV/mm | 382 kV/in | ASTM D149 |
Devcon Sprayable Ceramicâ„¢ Epoxy Precision Repair EpoxyComments: A sprayable ceramic-reinforced composite that can be sprayed in a manner similar to high-solid paints. Ideal for protecting pumps, paper machines, stacks, pump pads,.. |