Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 15.3 kV/mm | 389 kV/in | ASTM D149-97a |
DSM Somos® WaterClear® 10110 Epoxy Resin for Stereolithography
(discontinued **) DescriptionDSM Somos® 10110 is a high-speed liquid photopolymer that produces strong, rigid, and durable parts with optical clarity using stereolithography machines. This material is especially us.. |
|||
Dielectric Strength | 15.3 kV/mm | 389 kV/in | Short Time; ASTM D149 |
Plenco 1510 Polyester, Pellet, Injection Molded PLENCO 01510 is a mineral filled, pelletized polyester molding compound, which offers an excellent combination of electrical properties and dimensional stability. UL recognized under component file .. |
|||
Dielectric Strength | 15.3 - 17.3 kV/mm | 389 - 439 kV/in | short time |
Bulk Molding Compounds BMC T15(F) High Strength Grade Molding Compound BMC T15F is a high strength, low shrink general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T15F is well suited for injection, transfer or compression molding.. |