Dielectric Strength 155 kV/mm
3940 kV/in
ASTM D149
Ineos Styrenics Avantra® 585K Q402 Rubber Modified Polystyrene
Avantra® 585K Q402 is a high-impact grade of polystyrene with extremely high surface gloss and excellent practical toughness. Although Avantra® 585K Q402 can be processed by any method applic..
Dielectric Strength 155 kV/mm
3940 kV/in
ASTM D149
Ineos Styrenics Avantra® 585K Rubber Modified Polystyrene
Avantra® 585K is a high-impact grade of polystyrene with extremely high surface gloss and excellent practical impact strength. Although Avantra® 585K can be processed by any method applicable..
Dielectric Strength 155 kV/mm
3940 kV/in
K20/P50; IEC 60243-1
Styrolution Polystyrol 485 I GR 2 PS
Description: Polystyrol 485 I GR2 is a high-impact grade of polystyrene for extruded sheets with a matt surface.Applications: Sheet, semi finished goods, fat resistant food packaging.Information pro..
Dielectric Strength 155 kV/mm
3940 kV/in
K20/P50; IEC 60243-1
Styrolution Polystyrol 486 M GR 2 PS
Description: Polystyrol 486 M is a normal flowing, high-impact grade that is especially suitable for blends with a high proportion of general-purpose Polystyrol (preferably Polystyrol 165 H or Polys..
Dielectric Strength 155 kV/mm
3940 kV/in
K20/P50; IEC 60243-1
Styrolution Polystyrol 495 F GR 2 PS
Description: Polystyrol 495 F is a high impact polystyrene with a good heat resistance and high stiffness.Applications: Consumer electronics; TV-front and back; chassis for VCR and CD player. Househ..
Dielectric Strength 155 kV/mm
3940 kV/in
K20/P50; IEC 60243-1
Styrolution Polystyrol ESCRimo PS
Description: Polystyrol ESCRimo is a high-impact polystyrene grade with an improved stress cracking resistance compared to conventional high-impact polystyrene.Applications: Due to its superior envi..
Dielectric Strength 155 kV/mm

@Thickness 1.50 mm
3940 kV/in

@Thickness 0.0591 in
Short Time; IEC 60243-1
Styrolution PS 2710 HIPS
Styrolution PS 2710 is a high impact grade of polystyrene with improved stress crack resistance, developed for extrusion and thermoforming applications, especially for the refrigerator industry.Impr..
Dielectric Strength 155 kV/mm

@Thickness 1.50 mm
3940 kV/in

@Thickness 0.0591 in
Short Time; IEC 60243-1
Styrolution PS 456EB HIPS
Styrolution PS 456EB is a high flow, high impact polystyrene with a good heat resistance and a high stiffness, developed for injection blow molding applications, especially for bottle of yot.High fl..
Dielectric Strength 155 kV/mm

@Thickness 1.50 mm
3940 kV/in

@Thickness 0.0591 in
Short Time; IEC 60243-1
Styrolution PS 476L HIPS
Styrolution PS 476L is a normal flow and very high impact Polystyrene. It gives good mechanical and heat resistance properties while providing with easy processability and short cycle time.Normal fl..
Dielectric Strength 155 kV/mm

@Thickness 1.50 mm
3940 kV/in

@Thickness 0.0591 in
Short Time; IEC 60243-1
Styrolution PS 495F HIPS
Styrolution PS 495F is a high flow, high impact polystyrene with a good heat resistance and a high stiffness.High flow HIPSGood heat resistance with high stiffnessSuitable for gas-assisted injection..
Dielectric Strength 155 kV/mm

@Thickness 1.50 mm
3940 kV/in

@Thickness 0.0591 in
Short Time; IEC 60243-1
Styrolution PS 576H HIPS
Styrolution PS 576H is a high gloss, high impact polystyrene with a good flow and good heat resistance.High gloss HIPSGood flow and heat resistanceHIPS with good balance of mechanical properties and..