Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 17.4 kV/mm | 441 kV/in | |
Dow Corning HV 1660/65 LIGHT GRAY SILICONE RUBBER KP 65 Shore hardness high consistency silicone rubber with excellent tracking and erosion resistance, excellent wet electrial properties,high voltage insulation applications.Information provided by Dow.. |
|||
Dielectric Strength | 17.4 kV/mm | 441 kV/in | Arlon SQA-TMS-020 |
Arlon 55986C028 0.0295" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave 1: N/ASide 1: Cured Silicone RubberSubstrate: Style 162 FiberglassSide 2: Uncured Silicone RubberInterleave 2: LDPEThis data represents typical values for the pro.. |