Electrical Properties Metric English Comments
Dielectric Strength 18.8 kV/mm

@Thickness 3.20 mm
478 kV/in

@Thickness 0.126 in
in oil; ASTM D149
SABIC Innovative Plastics NORYL PX9406 PPE+PS
Nonbrominated, nonchlorinated, flame retarded. Improved productivity and reliability. 252F HDT. UL94 V-0 rated. Electrical applications.
Dielectric Strength 18.8 kV/mm

@Thickness 3.20 mm
478 kV/in

@Thickness 0.126 in
in oil; ASTM D149
SABIC Innovative Plastics NORYL PX9406 PPE+PS (Asia Pacific)
Nonbrominated, nonchlorinated, flame retarded. Improved productivity and reliability. 252F HDT. UL94 V-0 rated. Electrical applications.
Dielectric Strength 18.8 kV/mm
478 kV/in
Covestro Desmopan® 487 Thermoplastic Polyurethane
Desmopan 487 is a TPU on the basis of a special ester.Applications: Seals, gear wheels, shoe heels, engineering components in the automotive sector.Information provided by Bayer.As of 1 September 20..