Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 19.3 kV/mm | 489 kV/in | ASTM D149 |
Arlon 55578R028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: LDPESide 2, Layer 2: Uncured Silicone Rubber Side 2, Layer 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Side 1: Silicone Skim Coat Appearance: Red silico.. |