Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 50.20 kV/mm | 1275 kV/in | ASTM D149 |
Arlon R37292S018 0.018" (0.457 mm) Cured Silicone Rubber with PTFE Coated Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 1: Cured Silicone RubberCarrier: PTFE Coated FiberglassThis data represents typical values for the production material. The data should not be used .. |