Polymer Property : Dielectric Strength = 5000 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 19.7 - 197 kV/mm
500 - 5000 kV/in
Average value: 96.8 kV/mm Grade Count:7
Overview of materials for Fluorocarbon ETFE/ECTFE, Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Fluorocarbon ETFE/ECTFE, Molded/Extruded". Each property range of values reported is minimum and maximum..