Dielectric Strength 51.77 kV/mm
1315 kV/in
Saint-Gobain CHR® M717 Polyester Film Backing Silicone Adhesive Pressure Sensitive Tape
Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa..