Electrical Properties Metric English Comments
Dielectric Strength 22.9 kV/mm

@Thickness 2.00 mm
582 kV/in

@Thickness 0.0787 in
in oil; IEC 60243-1
SABIC Innovative Plastics NORYL WCD933 PPE-TPE
Flexible and non-halogenated flame retardant extrusion grade intended for evaluation in applications such as insulation of HD 21.14 flexible cables. Flame retardant performance capable of meeting EN..
Dielectric Strength 22.9 kV/mm

@Thickness 2.00 mm
582 kV/in

@Thickness 0.0787 in
in oil; IEC 60243-1
SABIC Innovative Plastics NORYL WCD933 PPE-TPE (Asia Pacific)
Flexible and non-halogenated flame retardant extrusion grade intended for evaluation in applications such as insulation of HD 21.14 flexible cables. Flame retardant performance capable of meeting EN..
Dielectric Strength 22.9 kV/mm

@Thickness 2.00 mm
582 kV/in

@Thickness 0.0787 in
in oil; IEC 60243-1
SABIC Innovative Plastics NORYL WCD933 PPE-TPE (Europe-Africa-Middle East)
Flexible and non-halogenated flame retardant extrusion grade intended for evaluation in applications such as insulation of HD 21.14 flexible cables. Flame retardant performance capable of meeting EN..