Electrical Properties Metric English Comments
Dielectric Strength 6.30 kV/mm
160 kV/in
Step by Step; ASTM D149
Plenco 00714 Melamine-Phenolic, Granular, Injection Molded
PLENCO 00714 is a melamine-phenolic copolymer molding compound, offering excellent arc resistance and comparative track index values. Type ASTM D 5948 CMG, and UL recognized under component file E4..
Dielectric Strength 6.30 kV/mm
160 kV/in
Aremco Ceramacoat™ 512-N High Temperature Potting & Casting Material Silica
Viscous, off-white paste for circuit breakers, power resistors and solenoids to 240°F (1316°C)
Dielectric Strength 6.30 kV/mm
160 kV/in
Short Time; ASTM D149
Plenco 7591 Phenolic, Pellet, Transfer Molded
PLENCO 07591 is a mineral and flock cotton filled novolac phenolic molding compound. UL recognized under component file E40654.Information supplied by Plenco.