Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Dielectric Strength = 632 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 24.9 kV/mm

@Thickness 3.00 mm
632 kV/in

@Thickness 0.118 in
IEC 243
Sumitomo Bakelite North America RX® 660 Fiberglass Reinforced Phenolic Novolac
RXÂ 660 is a fiberglass reinforced phenolic molding compound, with good dimensional stability and good strength at elevated temperatures. Meets ASTM D-5948 Type MFH.Information supplied by Sumitom..