Electrical Properties Metric English Comments
Dielectric Strength 25.1 - 26.2 kV/mm
638 - 665 kV/in
DC Breakdown Strength
China-Yixing Longly Refractories ZTA (20%ZrO2) Zirconia Toughened Alumina Composite Ceramic
LONGLY's Zirconia Toughened Alumina ceramics (hereafter referred as composite ceramic, ZTA) is white, corrosion resistance, good chemical stability. As well all know that alumina is hard, while zir..
Dielectric Strength 25.1 kV/mm
638 kV/in
ASTM D149
Arlon 55576R060 0.060" Cured/Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 162 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PEThis data represents typical values for the production material ..