Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 25.7 kV/mm @Thickness 1.60 mm |
653 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics NORYL PX1007 PPE+HIPS (Europe-Africa-Middle East) NORYL* PX1007 is an unfilled non-chlorinated, non-brominated flame retardant PPE/HIPS grade, targeted for flat panel TV enclosures. It has a Vicat B/120 temperature of 96 degC and UL-94 V0 @ 1.5mm .. |
|||
Dielectric Strength | 25.7 kV/mm | 653 kV/in | |
Dow Corning Q2-7406 ADHESIVE Dow Corning® Q2-7406 Adhesive is a polydimethylsiloxane gum and resin dispersion; provides excellent high temperature properties with adhesion to 288C (550F).Information provided by Dow Corning |