Polymer Property : Dielectric Strength = 76.0 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 76.0 kV/mm

@Thickness 0.0762 mm
1930 kV/in

@Thickness 0.00300 in
ASTM D149
Westlake Plastics PVDF Film Made from KYNAR® Polyvinylidene Fluoride Resin
Excellent chemical resistance. Stable to UV and the effects of weather. Low NBS smoke generation and superior LOI. Excellent transmittance of solar energy. Excellent dielectric strength. High h..