Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 8.64 kV/mm | 219 kV/in | |
GBC 496 Alumino Silicate Ceramic Propriety composition with CTE equivalent to Pyrex® glass. Can seal directly to 7070 glass, Pyrex®, or other grades of silicon. Has excellent thermal shock resistance, low firing temperature.. |