Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 31.9 kV/mm | 810 kV/in | ASTM D149 |
ExxonMobil Santoprene® 251-70W232 Thermoplastic Elastomer A soft, colorable, flame retardant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material has good fluid resistance and contains non-ether brominated flame retard.. |