Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 34.1 kV/mm | 866 kV/in | |
Arkema Group Rilsan® AESN G9 T6L Nylon 12, Graphite Filled (Dry) Designation ISO 1874-PA12,EHLS,22-010,CD10Rigid grade with graphite fillers for extrusion. Available color: steel gray. Reinforced light and heat stabilizing agents.Very low friction coefficient. No.. |
|||
Dielectric Strength | 34.1 kV/mm | 866 kV/in | ASTM D149 |
Arlon 915-20R##-P0 0.015" (0.381 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 2” Wide Rectangular 2 inch wide, 15 mil thick, Red, Rectangular cross-section, Self-fusi.. |