Polymer Property : Dielectric Strength = 881 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 34.7 kV/mm
881 kV/in
Tape Property; ASTM D149
Arlon SFT 0.012" (0.305 mm) Cured Self-fusing Silicone Tape
Design/Construction: Interleave: PET Product: Cured Self-Fusing Silicone Rubber Cross-Section: 1” Wide RectangularDescription: 1 inch wide, 12 mil thick x 10 yards long, Gray, Rectangular cross-sec..