Polymer Property : Dielectric Strength = 99.1 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 3.90 kV/mm
99.1 kV/in
IEC 60243
Solvay TECHNYL® 1011R PA6, Conditioned
Description: Polyamide 6, Unfilled, lubricated, for injection molding. Available in: Asia Pacific Product Applications: TECHNYL® 1011R is used in all sectors of industry, offering an excellent flow..