Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 0.0000188 ohm-cm @Temperature 0.000 - 100 °C |
0.0000188 ohm-cm @Temperature 32.0 - 212 °F |
|
H.C. Starck NRC® 91 Tantalum - 7% Tungsten Alloy Applications: NRC® 91 Metal wire products are primarily used for their superior tensile and yield strengths and torsion modulus. These properties are retained at high temperatures in vacuum. F.. |