Polymer Property : Volume Resistivity = 0.000092 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 0.000092 ohm-cm
0.000092 ohm-cm
ATI Allegheny Ludlum AL 4565™ Corrosion Resistant Stainless Steel
Characteristics:Very high resistance to pitting and crevice corrosion Excellent general corrosion resistance in a variety of media Higher mechanical propertied then conventional stainless steels Go..