Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 0.00017 ohm-cm | 0.00017 ohm-cm | cured 15 min @ 150°C |
Tra-Con Tra-Duct 921M01 Low Viscosity Long Pot Life Silver-Filled Epoxy TRA-DUCT 921M01 is a two component, silver-filled electrically conductive epoxy adhesive designed for applications which require electrical conductivity and a long pot life at a relatively low heat .. |