Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 0.0014 ohm-cm | 0.0014 ohm-cm | |
SGL Carbon Group SIGRAFIL C® C30 T050 EPY Continuous Tow Carbon Fiber with 50k filaments, Epoxy Sizing SIGRAFIL C as continuous tow is ideal for waving, prepregging, filament winding, Carbon Fiber Reinforced Plastics (CFRP) components, advanced composites, multi-axial production, unidirectional tapes.. |
|||
Volume Resistivity | 0.0014 ohm-cm | 0.0014 ohm-cm | Cured: 24 hours at 25°C |
Resinlab® SEC1222 Silver Filled Epoxy Adhesive Resinlab™ SEC1222 is a silver filled, two component, room temperature curing epoxy adhesive. It is designed to cure completely at room temperature. SEC1222 provides excellent electrical conductivit.. |