Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 0.70 ohm-cm | 0.70 ohm-cm | |
Cotronics Duralco™ 122 500°F (260°C) Nickel Filled Adhesive and Casting Epoxy Specially formulated to provide an economical alternative to silver filled electrically conductive epoxies. Applications: for use in applications where highest electrically conductivity not required.. |